The production process of Ceramic foundry sand

Ceramic sand is produced by adding the electric arc furnace containing Al2O3 45%-90% raw bauxite ore, the high temperature produced by the arc of the arc discharge, the raw material bauxite melted liquid, the liquid flows out of the furnace, impose its 70-85m/s to air pressure, the liquid material with the strong wind crushing, cooled to obtain spherical or nearly spherical shape, smooth sand performance.

mic casting sand ceramic casting sand ceramic casting sand ceramic casting sand

Grain type

ball, spherical

Angularity

1.1 max, similar to ball

Bulk density

1.95-2.05 g/cm3

Refractoriness

1790℃

Thermal expansion

0.13% (10 min at 1000 C )

Size

Available in all models, it can also be customized

 

Composition

Content

Al2O3

70-75%

SiO2

8-20%

Fe2O3

≤ 3%

TiO2

≤ 3.5 %

CaO

≤ 0.45 %

MgO

≤ 0.35 %

K2O

≤ 0.33%

Na2O

≤ 0.08 %